MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultraform® S 2320 003 BK120 Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Ultraform® S 2320 003 BK120 Q600 is a pigmented black, easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. Typical applications include difficult, thin-walled parts.

Availability: North America

Additive: Mold Release

Features: Copolymer; Good Flow; Good Mold Release

Use: Thin-walled Parts

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black

Forms: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Water Absorption 0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %ISO 62
Maximum Moisture Content 0.15
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4790 psi
@Temperature 80.0 °C
ISO 527-2
 9430 psi
@Temperature 22.8 °C
ISO 527-2
 13500 psi
@Temperature -40.0 °C
ISO 527-2
Elongation at Break 28 %Nominal; ISO 527-2
Elongation at Yield 9.0 %ISO 527-2
Tensile Modulus 392000 psiISO 527-1
Charpy Impact, Notched 2.40 ft-lb/in²
@Temperature -30.0 °C
ISO 179
 2.60 ft-lb/in²
@Temperature 22.8 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 100 Hz
IEC 60250
 3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 61.0 µin/in-°FISO 11359-2
Melting Point 333 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 212 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 374 - 446 °F
Mold Temperature 140 - 248 °F
Drying Temperature 176 - 230 °F
Dry Time 2.00 - 4.00 hour
Injection Pressure 508 - 1020 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2124 / 310817

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.