MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mercury Indium Selenide, HgIn2Se4
Categories: Ceramic; Sulfide/Chalcogenide; Other Engineering Material; Semiconductor

Key Words: Chalcogenide; Semiconductor; Selenium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.30 g/cc0.228 lb/in³
a Lattice Constant 5.764 Å5.764 Å
c Lattice Constant 11.8 Å11.8 Å
 
Electrical PropertiesMetricEnglishComments
Band Gap 0.60 eV0.60 eV
Electron Mobility, cm²/V-s 290290
 
Thermal PropertiesMetricEnglishComments
Melting Point 827 °C1520 °F
Heat of Formation 196 kJ/mol196 kJ/mol
 
Descriptive Properties
Crystal StructureTetragonal"Defect Chalcopyrite" Structure - Space Group I(-4)

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mercury (II) Oxide, HgO (Montroydite)
Mercury Aluminum Selenide, HgAl2Se4
Mercury Aluminum Sulfide, HgAl2S4
Mercury Gallium Selenide, HgGaSe4
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled

DSEN20 / 3033

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.