MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R 770/75 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 770/75 is a peroxide crosslinking HCR silicone for the manufacture of flame retardant profiles.

Properties: The color of the rubber base is white. Therefore, colors will not match the RAL color codes of the masterbatches used in paste or pellet form in the compound (pastel colors). Apart from its low inflammability the 50 Shore A version exhibits high mechanical strength. The 70 Shore A version shows an extremely high oxygen index (LOI), and, at a thickness of 2 mm it may pass the test according to UL 94 V0.

Special features:

  • flame retardant
  • tested according to BS 6853 category 1
  • tested according to London Underground standards
  • high temperature index
  • low toxicity combustion products generating low quantity of smoke
  • good mechanical properties

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183-1 A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7676DIN 53505
Tensile Strength at Break 4.10 MPa595 psiDIN 53504 S1
Elongation at Break 220 %220 %DIN 53504 S1
Tear Strength 16.0 kN/m91.3 pliASTM D624 B
Compression Set 39 %39 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN IEC 93
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) >= 35 %>= 35 %ASTM D2863
 
Descriptive Properties
Appearancewhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering S50R Silicone Rubber
NuSil LSR-5850 Liquid Silicone Rubbers (LSR)
Momentive Performance Materials Addisil™ 1070 E Industrial Extrusion Heat Cured Rubber
LG Chemical 1.3-Butadiene
KKPC KOSYN KSL 341 Styrene-Butadiene Latex

PWACK9242 / 204771

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.