Production Description: Topolymer® 9210-751 is a heat stabilized PP/EPDM based Thermoplastic Vulcanized Elastomer(TPV). This compound is intended for use in a wide range of applications such as gaskets, seals, covers, electronics or other parts where softness and conformity are needed. 9210-751 can be processed using Injection Molding, Extrusion, Blow molding or other melt processing techniques. Features: - Good resistance to ozone and excellent flex fatigue resistance.
- EU and China RoHS compliant.
- It is polyolefin based and completely recyclable.
Application: Light colour, easy coloring. Recommended for applications requiring excellent flex fatigue resistance, excellent ozone resistance. Used in interior, encapsulation applications and sealing applications. These grades of Topolymer TPVs can be processed on conventional thermoplastics equipment for injection molding, extrusion or blowmolding.Information provided by Top Polymer Enterprise |