MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Pressure Seal 5752 Nitrile - Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 5752 is a 70 durometer purple colored Buna N elastomer. It exhibits good physicals and good resistance to petroleum based oils at moderate temperatures.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 720 EO14 EO34; 2 BG 720 EF11 EO14 EO34; 3 BG 720 B14 EO14; 4 BG 720 B14 EO14; 5 BG 720 A14 EO14 EO34; 4 BK 720 A24 EF11

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 69
 52
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 57
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 61
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3
 66
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 69
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1
 71
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 71
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 73
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged
Tensile Strength 2291 psi
 817.9 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 1420.4 psi
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged
 2032.1 psi
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 2032.1 psi
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 2176.5 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 2201.65 psi
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3
 2703.4 psi
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1
Elongation, Ultimate 868 %
 261.3 %
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged
 535.6 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 622.4 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3
 646.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1
 715.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 715.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 808.1 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
100% Modulus 379 psi
Tear Strength 153 pliDie B
 208 pliDie C
Compression Set 39.6 %
@Treatment Temp. 100 °C,
Time 79200 sec
Solid
 46.2 %
@Treatment Temp. 100 °C,
Time 79200 sec
Plied
 51.9 %
@Treatment Temp. 100 °C,
Time 252000 sec
Solid
 60.4 %
@Treatment Temp. 100 °C,
Time 252000 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -12.0 °F
Shrinkage -4.20 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, ASTM Oil #1
 2.2 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 7.4 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, ASTM Oil #3
 8.8 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 30.9 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 
Descriptive Properties
ColorPurple

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL045 / 318255

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.