MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Good Elasticity – High melt flow for easy processing

Uses: Extrusion – Wire and cable, general extrusion

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
82 - 88
@Time 0.00139 hour
ASTM D2240
Tensile Strength 40.7 MPa5900 psiASTM D412
Elongation at Break 600 %600 %ASTM D412
100% Modulus 6.90 MPa
@Strain 100 %
1000 psi
@Strain 100 %
ASTM D412
300% Modulus 11.0 MPa
@Strain 300 %
1600 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0410 GPa5.94 ksiASTM D790
Tear Strength 22.8 kN/m130 pliTrouser; ASTM D470
Graves Tear Strength 66.6 kN/m380 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4.54.5CS-17, 1000g; ASTM D3389 B
Compression Set  20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
 66 %
@Temperature 70.0 °C,
Time 79200 sec
66 %
@Temperature 158 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -50.0 °C-58.0 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 174 °C345 °FExtrusion
Zone 2 180 °C356 °FExtrusion
Zone 3 188 °C370 °FExtrusion
Zone 4 194 °C381 °FExtrusion
Adapter Temperature 194 °C381 °F5, Extrusion
Die Temperature 185 °C365 °FZone 2, Extrusion
 191 °C376 °F6, Zone 1, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane

PNOVEON055 / 55322

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.