MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Bicor® 120 LTSC OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTSC) delivers a low seal initiation temperature. LTSC provides a forgiving, wide operating range for applications where accurate heat control is a problem, or dwell times vary because of frequent machine speed changes. LTSC’s acrylic surface is excellent for surface printing and provides good aroma barrier.

Availability: Latin America, North America and South America

Key Features:

  • Wide sealing range with a low minim seal temperature (MST)
  • Excellent seal strength and hot tack
  • Robust performances on horizontal flowpack machines
  • Excellent humidity seal retention on LTSC side
  • Good flavor and aroma barrier
  • Outstanding optical properties
  • Ideal support for normal ink systems
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • Humidity Resistant
  • In Lamination Lap Sealable
  • LTS Coated
  • Very Broad Seal Range
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Frozen Food
  • Health and Beauty Care
  • Household and Detergents
  • Tobacco
Uses:
  • HFF Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 5.00 g/m²/day
@Temperature 38.0 °C
0.322 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Thickness 30.5 microns1.20 milNominal; ExxonMobil Method
Coating Weight 27.0 g/m²16.9 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.240.24ExxonMobil Method
Film Tensile Strength at Break, MD 138 MPa20000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 228 MPa33000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
5.0 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 4.5 %
@Temperature 135 °C
4.5 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.2 %2.2 %ExxonMobil Method
Gloss 90 %90 %45º, Acrylic Surface; ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST160°FLTSC/LTSC, 200g/in
Crimp Seal Strength590 g/inLTSC/LTSC, 260°F, 20psi, 3/4sec
Yield25500 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer

PEXB388 / 37693

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.