MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Latrobe Lescalloy® HY-180 VIM-VAR ; 2.01 - 4.00 thickness High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superior cleanliness and ingot homogeneity, and to enhance mechanical properties.

Mechanical Properties from FMS-1111 Specification

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1310 MPa190000 psi
Tensile Strength, Yield 1207 MPa175100 psi
Elongation at Break 12 %12 %
Reduction of Area 60 %60 %
Modulus of Elasticity 190 GPa27600 ksi
Charpy Impact 68.0 J
@Temperature -17.8 °C
50.2 ft-lb
@Temperature 0.000 °F
V-notch
 
Processing PropertiesMetricEnglishComments
Processing Temperature 166 °C331 °FCritical Temperaure Mf
 327 °C621 °FCritical Temperaure Ms
 624 °C1160 °FCritical Temperaure Ac1
 793 °C1460 °FCritical Temperaure Ac3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.13 %0.13 %
Chromium, Cr 2.0 %2.0 %
Cobalt, Co 8.0 %8.0 %
Iron, Fe 78.72 %78.72 %
Manganese, Mn 0.10 %0.10 %
Molybdenum, Mo 1.0 %1.0 %
Nickel, Ni 10 %10 %
Silicon, Si 0.050 %0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel

NTIMK021 / 19369

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.