MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Sulfur
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Like many oil resistant synthetic rubbers, Millathane 76 requires a treated grade of sulfur to ensure proper dispersion.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
Tensile Strength 4809 psi
Elongation at Break 588 %
100% Modulus 0.480 ksi
@Strain 100 %
200% Modulus 1.082 ksi
@Strain 200 %
300% Modulus 1.909 ksi
@Strain 300 %
Tear Strength 59.7 kN/mDie C
Compression Set 27.1 %
@Temperature 70.0 °C,
Time 79200 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 8.80 min
@Temperature 155 °C
TC90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mearthane Durethane™ M DM-650A Foam Polyurethane
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.5 PHR Sulfur
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Mearthane Durethane™ S DS-210A Solid Polyurethane Elastomer
TSE Industries Millathane® 66 Millable Polyurethane Rubber

PMILL013 / 87057

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.