MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cabot PLASBLAK® XP6784A Black masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: PLASBLAK XP6784A black masterbatch is suitable for use in irrigation pipes and geomembranes. It contains a carbon black that provides superior protection against UV light degradation, as well as a highly efficient stabilization package that can enable excellent long term thermal and process stability.

Method of addition: PLASBLAK XP6784A black masterbatch is designed for ease of dilution and homogeneous mixing and is therefore suitable for direct addition using automatic dosing units or by pre-blending.

Addition rate: The amount of masterbatch added depends on the performance requirements of the final application. For effective protection against the effects of UV exposure, a masterbatch addition rate of 6.25% is typical.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D-792
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D-1238
 
Descriptive Properties
AdditiveAntioxidant
CarrierPE
CompatibilityLLDPE, MDPE, HDPE, PP
Pigment40% carbon black (with superior UV performance)
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT010 / 315745

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.