MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TBA ECP 2368 Static Dissipative Colorable ABS Injection Molding Compound
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: ECP 2368 is a proprietary TBA injection molding compound utilizing a special non-migratory additive system to give a permanently static dissipative material. The material is specially designed for applications requiring static control such as electronic safe handling areas and hazardous environments. Used for anti static applications where ESD (electro static discharge) is to be avoided.

Applications:

  • Production aids for the electronics industry (eg, storage boxes, bins, trays)
  • Audio/hi-fi accessories
  • Static dissipating equipment housing

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 23.0 MPa3340 psiISO 527
Tensile Modulus 1.30 GPa189 ksiISO 527
Flexural Modulus 1.30 GPa189 ksiISO 178
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1.00e+9 ohm<= 1.00e+9 ohmDIN 53482
Static Decay <= 0.25 sec<= 0.25 sec5000/50V; FTMS-101C
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.050 - 0.070 %0.050 - 0.070 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 230 °C392 - 446 °FCylinder
Mold Temperature 25.0 - 50.0 °C77.0 - 122 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTBA015 / 281493

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.