MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
High-leaded brass, UNS C34200, H02 Temper rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Combines excellent machinability with moderate cold workability.

Applications: gears, pinions, valve stems.

Test specimen: rod - 25mm diameter.

Key Words: CZ119, ISO CuZn35Pb2, CEN CW601N, free-cutting brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 72
Tensile Strength, Ultimate 450 MPa
Tensile Strength, Yield 310 MPa
Elongation at Break 23 %In 50 mm, Reduction in area 35%
Modulus of Elasticity 105 GPa
Poissons Ratio 0.346
Machinability 90 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 885 - 910 °C
Solidus 885 °C
Liquidus 910 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 785 - 815 °C
Recrystallization Temperature 320 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 62.5 - 66.5 %
Iron, Fe <= 0.10 %
Lead, Pb 1.5 - 2.5 %
Other, total <= 0.50 %
Zinc, Zn 33.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-leaded brass, UNS C34200, H55 Temper rod
Beryllium Copper, UNS C17200, TB00 Temper rod, bar, plate, tubing
High-leaded brass, UNS C34200, OSO50 Temper rod
Leaded Copper, UNS C18700
Medium-leaded brass, UNS C34000, H02 Temper rod

MC34200c3 / 11211

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.