MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT Group QM 226 26 Shore A, Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 226 is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for moldmaking of intricate patterns, skin molding and applications where a low durometer material is required.

Key Features:

  • Low viscosity
  • Fast demold time
  • Excellent physical properties
  • Excellent flexibility
  • Excellent library life
Main Applications:
  • Special effects
  • Applications where low modulus is required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccQM 226B
 1.12 g/cc1.12 g/ccQM 226A
Viscosity 8000 cP8000 cPQM 226B
 17000 cP17000 cPCatalyzed
 20000 cP20000 cPQM 226A
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inCured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2626Cured
Tensile Strength 4.48 MPa650 psiCured
Elongation at Break 650 %650 %Cured
Tear Strength 15.8 kN/m90.0 pliCured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FCured
Minimum Service Temperature, Air -55.0 °C-67.0 °FCured
 
Processing PropertiesMetricEnglishComments
Cure Time 360 - 480 min6.00 - 8.00 hourDemold time, Catalyzed
Pot Life 30.0 min30.0 minCatalyzed
 
Descriptive Properties
ColorRedQM 226B, Uncatalyzed
 RedCatalyzed
 TranslucentQM 226A, Uncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
CHT Group True Skin® 30 30 Shore A, Clear Addition Cure Material
CHT Group QM 280 80 Shore A, Addition Cure Moldmaking Material
CHT Group QM 270 Green 70 Shore A, Addition Cure Moldmaking Material
CHT Group QM 261 60 Shore A, Addition Cure Moldmaking Material

PACC2046 / 199434

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.