MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnapas® 4021 T Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 4021 T is a copolymer powder of vinyl acetate and ethylene and is dispersible in water.

Properties: Compounds modified with VINNAPAS® 4021 T exhibit improved adhesion, flexural strength, deformability and abrasion resistance and are easier to process. Combinations with cement and gypsum can provide mortars which exhibit non-sag properties. VINNAPAS® 4021 T contains a fine mineral filler as an antiblocking agent. It is produced without the use of organic solvents, plasticizers and film-forming agents.

Special features: VINNAPAS® 4021 T is a non-slump dispersible polymer powder in the medium Tg range. It is suitable for formulating compounds that must exhibit good nonslump properties and low emissions.

Application: Typical applications for VINNAPAS® 4021 T: include blending with inorganic binders, such as cement, anhydrite, gypsum plaster and hydrated lime for the manufacture of adhesives, patching compounds, cement and lime-cement finish plasters and repair mortars.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.420 - 0.500 g/cc0.0152 - 0.0181 lb/in³DIN EN ISO 60
Solids Content >= 98 %>= 98 %
Particle Size 400 µm400 µmmax 4% over; DIN EN ISO 4610
Ash <= 11.2 %<= 11.2 %
 
Descriptive Properties
Appearancewhite to light beige powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9601 / 205130

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.