MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CP-Polymer-Technik Wellamid® 6600/506 HWCP Nylon 66, Impact Modified, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Information provided by CP-Polymer-Technik GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.5 - 3.0 %2.5 - 3.0 %23°C/50%RH; DIN 53495
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm
@Thickness 4.00 mm
0.0080 - 0.012 in/in
@Thickness 0.157 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 75.0 MPa10900 psi50 mm/min; ISO 527
Elongation at Break 20 %20 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.70 GPa392 ksiISO 527
Flexural Modulus 2.20 GPa319 ksiDIN 52457
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.24 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohm1.00e+13 ohmISO 3915
Dielectric Constant 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 243-1
Dielectric Loss Index 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 V600 VStufe; IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 53752
Melting Point 255 °C491 °FKofler
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FISO 179
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 179
Vicat Softening Point 200 °C392 °F50 N; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Stufe; IEC 707
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Stufe; IEC 707
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 50.0 - 90.0 °C122 - 194 °F
 
Descriptive Properties
Back PressureLow
Holding PressureHigh
Injection SpeedMedium to High
Screw SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Conditioned
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned

PWELL124 / 72581

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.