MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Armacell ArmaSport® MLC-2 Continuous Rolls, PVC/NBR
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Armacell makes a wide range of closed-cell Component Foam materials for personal flotation devices (PFD). ArmaSport® MLC-LP, a low phthalate, UL Listed foam suitable for use in children’s life vests, pool floats and water accessories.

Product Advantages:

  • Moisture resistant closed cell structure
  • UL Listed
  • Low density / high buoyancy
  • Designed for vinyl coating
  • Tough skin for improved performance
  • Natural color, covers easily
  • Industry Leading Technical Support
  • Made in USA
MLC-LP Added Benefits
  • Low phthalate, CPSIA Compliant
  • Suitable for children’s applications
Recommended Applications
  • Pool, lake and ocean floats
  • Life vests and jackets
  • Water toys and accessories
  • For marine and leisure use
  • Options for adults and children

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 - 4.50 lb/ft³ASTM D1056
Water Absorption <= 7.0 %ASTM D1056
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 40.0 psiASTM D412
Elongation at Break >= 125 %ASTM D412
Compressive Strength 1.50 - 3.50 psi
@Strain 25 %
ASTM D1056
Compression Set <= 30 %
@Strain 50 %
ASTM D1056
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °FIntermittent; ASTM D1056
Minimum Service Temperature, Air -30.0 °FCold Crack; ASTM D1056
 
Descriptive Properties
ColorNatural
Flammability0 Burn Rate@ 1/8" No Skin, FMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Klinger Thermoseal ML-5270 PTG Gasketing
Armacell ArmaSport® MFC-2 Continuous Rolls, PVC/NBR
Armacell ArmaSport® MC Continuous Rolls, PVC/NBR
Karina E 85/201-DA-IS-SI Clear PVC Compound
Karina 85/201-DA-IS-SI-AT Clear PVC Compound

PARMD046 / 186657

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.