MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tritan™ LX201 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan LX201 was developed for the cosmetic, fragrance, and personal care markets. Tritan LX201 can easily be converted into articles for application in Consumer and Personal Care markets by injection molding, extrusion blow molding, and injection blow molding.

Application/Uses

  • Cosmetics hot-fill packaging
  • Cosmetics/personal care packaging
  • Fragrance packaging

Key Attributes

  • Ease of Processing
  • Excellent clarity
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Outstanding impact resistance

Typical properties as reported are preliminary. Information was provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D785
Tensile Strength at Break 53.0 MPaASTM D638
Tensile Strength, Yield 44.0 MPaASTM D638
Elongation at Break 140 %ASTM D638
Elongation at Yield 7.0 %ASTM D638
Tensile Modulus 1585 MPaASTM D638
Flexural Yield Strength 66.0 MPaASTM D790
Flexural Modulus 1585 MPaASTM D790
Izod Impact, Notched 126 J/m
@Temperature -40.0 °C
ASTM D256
 650 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 59.0 J
@Temperature 23.0 °C
Energy @ Max. Load; ASTM D3763
 63.0 J
@Temperature -40.0 °C
Energy @ Max. Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Transmission, Visible 92 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 282 °C
Mold Temperature 38.0 - 66.0 °C
Drying Temperature 88.0 °C
Dry Time 4 - 6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ TX2000 Copolyester
Eastman Tritan™ TX2001 Copolyester
Eastman Tritan™ MX810 Medical Grade Copolyester
Eastman Tritan™ FX100 Copolyester
Avient Edgetek® X TR2-20TA/000 NATURAL Copolyester

PE8912 / 109254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.