MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals SG90 Hydraulic Work Asphalt
Categories: Other Engineering Material

Material Notes: Hydraulic Work Asphalt: The hydraulic work asphalt takes low-wax and naphthene-base crude as raw material. The product features low wax, excellent anti-seepage performance, moderate composition and low brittle point. It has been successfully used in the large-scale (type 1) Class-Iproject - Shandong Yimeng Pumped Storage Power Station Upper Storage Reservoir Project. On October 31, 2021, the first No.1 andNo.2 units of Shandong Yimeng Pumped Storage Power Station were connected to improve the peak-shaving capacity of Shandongpower grid by 600,000kW. News 30’ on China Central Television reported the connection. The connection and operation of all four unitswill contribute to better peak-shaving capacity, power storage, and power supply at peak, saving 88,200 tons of standard coal, reducing296,700 tons of carbon dioxide emissions and 2,000 tons of sulfur dioxide emissions on a yearly basis. It will also play an active role instrengthening the regulation capacity of Shandong power grid, promoting energy transformation and achieving carbon peak & carbonneutrality, thus enabling “green power” grid connection in Shandong Province. Shandong Haiyun Asphalt Co., Ltd. has become the firstprivate company in the industry with engineering application achievements. Evaluated by Shandong Society of Chemistry and ChemicalEngineering, the technical achievements of the hydraulic work asphalt have reached the international advanced level.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Penetration 80 - 100
@Load 0.100 kg,
Time 5.00 sec
80 - 100
@Load 0.221 lb,
Time 0.00139 hour
[1/10mm]; GB/T 4509
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -12.0 °C<= 10.4 °FGB/T 4510
Flash Point >= 230 °C>= 446 °Fopen cup; GB/T 267
Ring & Ball Softening Point 45.0 - 52.0 °C113 - 126 °FGB/T 4507
 
Descriptive Properties
Content<2%Wax content (cracking), SH/T 0425
Ductility>150 cm5cm/min,15?, GB/T 4508
 >20 cm1cm/min,4?, GB/T 4508
Solubility>99%trichloroethylene, GB/T 11148

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB071 / 318613

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.