MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Multiflex™ TES A6221 CUV BLACK 28658 Styrenic Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Thermoplastic Elastomer based Styrenic

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
@Time 3.00 sec
ISO 7619-1
Tensile Strength at Break 8.00 MPaISO 527-1/-2
Elongation at Break 750 %ISO 527-1/-2
100% Modulus 2.30 MPa
@Strain 100 %
ISO 527-1/-2
Tear Strength 33.0 kN/mparallel; ISO 34-1
Compression Set 26 %
@Temperature 23.0 °C
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 °COptimum, Injection
Mold Temperature 20.0 - 60.0 °CInjection
 40.0 °COptimum, Injection
Back Pressure 1.00 MPa
 
Descriptive Properties
CompatibilityPolyolefins
Delivery formPellets
Drying Recommendedno
FeaturesHigh Flow
 High Gloss
Flow length (mm)850
Hold pressure rangeas low as possibleInjection
 as low as possibleInjection
Injection speedHigh
ProcessingFilm Extrusion
 Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDTF9359 / 254402

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.