MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Semicosil® 960 CLEAR Conformal Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: SEMICOSIL® 960 CLEAR is a RTV-1 amine cure silicone rubber dispersion that cures on contact with moisture in the air.

Special features:

  • Rapid cure
  • Excellent electrical properties
  • Excellent adhesion to many substrates
  • Available in clear or red
Application: SEMICOSIL® 960 CLEAR is a conformal coating that forms a tough, rubbery film designed to protect electronic circuits from environmental influences.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³
Solids Content 65 %65 %
Brookfield Viscosity 4000 cP4000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240
Tensile Strength at Break 1.72 MPa249 psiASTM D412
Elongation at Break 300 %300 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.7
@Frequency 1000 Hz
2.7
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243
Dissipation Factor 0.00030
@Frequency 1000 Hz
0.00030
@Frequency 1000 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Brittleness Temperature -45.0 °C-49.0 °FASTM D746
Flash Point 21.0 °C69.8 °FASTM D93
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Treatment Temp. 25.0 °C
168 hour
@Treatment Temp. 77.0 °F
50% RH
 
Descriptive Properties
AppearanceClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Semicosil® 960 RED Conformal Coating

PWACK9420 / 204949

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.