MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis Dutral® TER 4033 Ethylene - Propylene - Diene Terpolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Dutral® TER 4033 is an Ethylene - Propylene - Diene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.

Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® TER 4033 is a semi-crystalline, very low molecular weight terpolymer with medium diene content. Dutral® TER 4033 based compounds exhibit fast extrusion speed, fast curing and high state of cure, and it is particularly suitable in the production of high hardness extruded profiles (HHP). It can also be used to improve flow in compounds based on high molecular weight Dutral® grades.

Main Applications: Automotive, cables, mechanical goods, high hardness profiles.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.70 %<= 0.70 %
Mooney Viscosity 30
@Temperature 100 °C
30
@Temperature 212 °F
Ash <= 0.30 %<= 0.30 %
 
Descriptive Properties
ENB Content5% wt
Propylene Content25% wt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 12
Isoflon PMMA Polymethyl-methacrylate

PENG234 / 124628

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.