MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipol Technipol® PA 2167 Thermoplastic Adhesive Co-polyamide
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Technipol PA 2167 is a thermoplastic adhesive co-polyamide based for the automotive filter industry. It is characterized by a quick setting time, a good flexibility, a good wettability and a good chemical resistance. Technipol PA 2167 contains more than 80% of raw materials coming from renewable resources (not edible).

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D 792
Viscosity  3.0 cP
@Temperature 240 °C
3.0 cP
@Temperature 464 °F
 5.0 cP
@Temperature 220 °C
5.0 cP
@Temperature 428 °F
 7.0 cP
@Temperature 230 °C
7.0 cP
@Temperature 446 °F
 11 cP
@Temperature 200 °C
11 cP
@Temperature 392 °F
 30 cP
@Temperature 175 °C
30 cP
@Temperature 347 °F
Brookfield Viscosity 3.5 cP
@Temperature 232 °C
3.5 cP
@Temperature 450 °F
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 174 °C345 °FASTM D 3461
 
Processing PropertiesMetricEnglishComments
Processing Temperature 50.0 - 80.0 °C122 - 176 °FUnder Hopper
 150 - 170 °C302 - 338 °FCompression Zone
 180 - 200 °C356 - 392 °FMetering Zone
Feed Temperature 110 - 140 °C230 - 284 °F
Nozzle Temperature 190 - 210 °C374 - 410 °F
Die Temperature 180 - 200 °C356 - 392 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorAmber
Suggested temperature profile for melters185-195°CPre-Heating Grills
 190-210°CTank
 190-210°CHose
 190-210°CNozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL015 / 297140

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.