MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim X Gum Rosin
Categories: Other Engineering Material

Material Notes: Special Properties of Gum Rosin: Natural organic compound, mainly composed of resins, possesses chemical activity when dissolved in many organic solvents. Uses of Gum Rosin: At present, most rosin product is used for the manufacturing of paper, paint, soap and printing ink. Since rosin is easily softened and oxidized, in the oil paint industry, the carboxylation reaction of resin acid is usually employed to produce resinate for further use. While in the producing of synthetic rubber and printing ink, resin acid is changed into disproportionate rosin, polymerized rosin, hydrogenated rosin, etc for further use by its double bond reaction. Packing, Storing and Transporting of Gum Rosin: In galvanized Iron drums of about 225/230kgs net each, must be kept away from heat and flame.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash <= 0.020 %<= 0.020 %
 
Chemical PropertiesMetricEnglishComments
Acid Value >= 166>= 166[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point >= 76.0 °C>= 169 °F
 
Descriptive Properties
AppearanceTransparent
Colorslight yellow
Content<0.03%Insoluble Matter in Alcohol
 <5%Unsaponifiable Matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI110 / 317394

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.