System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ravago Manufacturing Americas Echo® RPH20TC BK Recycled Polypropylene Homopolymer, 20% Talc Filled
Categories:
Polymer
;
Renewable/Recycled Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 20% Talc Filler
Material Notes:
Post Consumer Homopolymer Propylene (Nylon content < 5%), 12 Melt Flow, 20% Talc Filled, Heat Stabilized, Black
Information provided by Ravago.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.10
g/cc
1.10
g/cc
ISO 1183
Melt Flow
8.0
-
16
g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0
-
16
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash
16 - 24 %
16 - 24 %
ISO 3451
Mechanical Properties
Metric
English
Comments
Tensile Strength
24.0
MPa
3480
psi
ISO 527
Flexural Modulus
2.00
GPa
290
ksi
ISO 178
Charpy Impact, Notched
0.200
J/cm²
0.952
ft-lb/in²
ISO 179-1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled
Overview of materials for Polypropylene with 20% Talc Filler
CTC X-PRO TF 1113 HP Polypropylene Homopolymer, 13% Talc Filled
Buckeye Polymers BP RPP 2012 T BLK Polypropylene, Talc Filled
Buckeye Polymers BP RPP 2007 TR Blk Reprocessed Polypropylene, 20% Mineral Filled
PENTA017m / 177141
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.