MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skamol Group Moler 10 Aggregate Insulation
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL insulating aggregates have the following characteristics:
  • Max. service temperature: Up to 900°C (1652°F)
  • Back-up insulation
  • Lightweight
  • Good insulating properties
  • Chemically inert
  • Due to free-flowing properties Moler aggregates are ideally suitable as a loose-fill insulation for furnace cavities and double skin linings, over arched roofs and in open joints, leveling of furnace bottoms and hearths.

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.449 g/cc0.0162 lb/in³As Supplied
Loss On Ignition 1.5 %
@Temperature 1025 °C
1.5 %
@Temperature 1877 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.160 W/m-K
@Temperature 200 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 392 °F
Mean temp.; BS 1902 Section 5.5 1991
 0.180 W/m-K
@Temperature 400 °C
1.25 BTU-in/hr-ft²-°F
@Temperature 752 °F
BS 1902 Section 5.5 1991
 0.200 W/m-K
@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1110 °F
BS 1902 Section 5.5 1991
Maximum Service Temperature, Air 900 °C1650 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 9.0 %9.0 %
CaO 0.80 %0.80 %
Fe2O3 7.0 %7.0 %
K2O 1.6 %1.6 %
MgO 1.3 %1.3 %
Na2O 0.40 %0.40 %
SiO2 77 %77 %
SO3 1.2 %1.2 %
TiO2 0.70 %0.70 %
 
Descriptive Properties
ColorRed-Brown
Pyrometric Cone Equivalent1350°CASTM C24-89, ORTON cones

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSKAM032 / 2183

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.