MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Master Builders Solutions ChemRex® CX Concrete Floor Primer - Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: CX Concrete Floor Primer is a waterborne epoxy primer for concrete substrates. It is designed to manage and reduce moisture vapor emission (out-gassing) of concrete slabs by controlling the rate of transmission through the permeance of the primer.

CX Concrete Floor primer is used on concrete floors and slabs, interior use, where low-odor applications are desired, where moisture vapor transmission of substrate exceeds 3 lb./1060 sq. ft./24 hours, and where vapor drive of porous concrete surfaces needs to be controlled.

The percent solid content is 51%. The drying time is 5 hours. The flash point is >200° given the ASTM D 93 test conditions. The VOC content is 118 g/L (0.99 lbs./gallon). The pull off strength after a 7 day cure is >300, depending on substrate. The coverage rate is 350-400 sq. ft. per gallon.

After one week CX Concrete Floor Primer is resistant to phosphoric acid (5%), acetic acid (5%), lactic acid (10%), diesel, motor oil, hydrogen peroxide, and salt water. After one week it is not resistant to nitric acid (5%), hydrochloric acid (10%), Sulfuric acid (10%), jet fuel, gasoline, and brake fluid.

Information provided by ChemRex, Inc.

Product of former ChemRex, Inc. BASF launched the Master Builders Solutions brand on January 15, 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 260
 
Mechanical PropertiesOriginal ValueComments
Taber Abrasion, mg/1000 Cycles 431000 g load (after a 7 day cure); ASTM D 4060-90
 
Optical PropertiesOriginal ValueComments
Gloss 62 %at 60° angle; TTS-141C method 6101.1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 °C
Pot Life 90 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Intex® 2740 Styrene - Butadiene Copolymer
Applied Nanotech Ag-iJ10 Silver Ink
Applied Nanotech Cu-iJ70P Copper Ink
Versalis Europrene Latice® 2430 Styrene - Butadiene Copolymer
Versalis Europrene Latice® 5570 Styrene - Butadiene Copolymer

PREX08 / 65567

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.