MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Zircar Refractory Composites RS-99-45 Refractory Sheet
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorganic binders. Type RS-99-45 has a high purity alumina bond making it well suited for use in high vacuum and reducing environments where silica cannot be tolerated, such as power metal and MIM furnaces with H2 atmospheres. It also has high electrical resistivity at elevated temperatures allowing it to be used in direct contact with resistance heating elements. It exhibits superior hot strength and dimensional stability to 1650°C (3000°F).

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.720 g/cc
Porosity 85 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00207 GPaparallel to thickness
Compressive Yield Strength 1.31 MPaat 10% compression, parallel to thickness
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 0.120 W/m-K
@Temperature 427 °C
 0.160 W/m-K
@Temperature 900 °C
 0.220 W/m-K
@Temperature 1200 °C
 0.290 W/m-K
@Temperature 1650 °C
Maximum Service Temperature, Air 1650 °C
Shrinkage 1.0 %
@Temperature 1200 °C,
Time 14400 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99 %
SiO2 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
DWA 6092/SiC/40p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
DWA 2009/SiC/25p-T4 Aluminum SiC Metal-Matrix-Composite (Al MMC)

CZRCI28 / 2891

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.