Description: PA6/ABS blend, injection molding grade. Black color. Suitable for parts requiring good dimensional stability, low warpage and good surface aspect. Good property retention after moisture absorption. Processing: Injection Molding Delivery Form: Granules Additives: Release agent Special Characteristics: Amorphous, High Surface Aspect, Low Moisture Absorption Industries: Automotive, Consumer Industry Goods, Transportation Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa Information provided by Radici Group |