MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Global EPP PA 6E Extruded Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecular chains. Their combined strengths and characteristics position them as obvious first choice materials for all components, subject to structural and wear conditions, in mechanical and plant engineering environments.

Key characteristics:

  • Excellent sliding and wear properties
  • Perfect balance of mechanical strength, toughness and rigidity
  • Good electrical insulating properties
  • Various FDA compliant grades available

This general-purpose grade offers an excellent blend of mechanical and impact strength, vibration damping and wear resistance. Complimenting these properties are good electrical insulation and favourable chemical resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.135 g/ccTest Method A; ISO 1183:1987
Moisture Absorption at Equilibrium 3.0 %50% RH; ISO 62:1999
Water Absorption at Saturation 9.5 %ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ISO 868:2003
Tensile Strength at Break 80.0 MPaSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 30 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 3.50 GPaSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 80.0 MPa1.5 mm/min; ISO 178:2001
Flexural Modulus 2100 MPa1.5 mm/min; ISO 178:2001
Compressive Strength 90.0 MPaSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 2600 MPaSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 8.00 kJ/m²Sample Type A; ISO 180:2000
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250:1969-01
 3.9
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mmIEC 60243-1:1998-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Thermal Conductivity 0.280 W/m-KISO 8301:1991
Melting Point 220 °C
Maximum Service Temperature, Air 90.0 °CContinuous
 160 °CIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 160 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75
Minimum Service Temperature, Air -40.0 °CContinuous
Glass Transition Temp, Tg 60.0 °CISO 11359-2:1999
Flammability, UL94 HBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorNatural, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SpinTech Veritex™ Shape Memory Polymer Composite
Firestone C200-001 Nylon 6
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
AISI 12L14 Steel, hot rolled, 19-38 mm round
Nitinol - NiTi Shape Memory Alloy; High-Temperature Phase

PGLOEPP00 / 79511

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.