MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Powersil® 79032 Silicone Dispersion
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: POWERSIL® 79032 is an electrically conductive silicone rubber dispersion in Xylene. POWERSIL® 79032 can be used as conductive coating and adhesion promoting primer. POWERSIL® 79032 comes ready-to-use as a 1- component system.

Special features:

  • electrically conductive coating
  • low volume resistivity
  • 1-component system
  • ready-to-use
  • adhesion promoting primer
Application:
  • cable accessories
  • electrodes
  • deflectors
  • adhesion promoter for molding RTV-2/LSR onto conductive silicone rubber

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cccured; ISO 1183-1 A
Solids Content 25 %
Brookfield Viscosity 250 cPMixing
 16000 cPdynamic
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.0 ohm-cmmeasure dry; IEC 60093
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Treatment Temp. 150 °C
circulating air oven
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Powersil® 570 Plus Silicone Insulator Coating
Wacker Powersil® 567 Silicone Insulator Coating
Wacker Powersil® 555 R Silicone Dispersion
Wacker Powersil® 552 Silicone Insulator Coating

PWACK9389 / 204918

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.