MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman PC/ABS CB1230K Polycarbonate
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC/ABS has ABS’ formability and PC’s mechanical resistance, impact strength, heat-resistance, resistance to ultraviolet (UV) and other features. Features: High rigidity and excellent anti-impact resistance Excellent heat resistance, Excellent processing performance, Excellent dimensional stability, Excellent weather resistance, Low-emission.

Applications: Dashboard skeleton, Tail lamp shell, Door handle, Window handle, Steering column sheath, Dashboard decorative box, Mirror shell.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in150*100*3.2 mm; PRET
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
20 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.0 MPa6670 psi50mm/min; ISO 527
Tensile Strength, Yield 53.0 MPa7690 psi50mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50mm/min; ISO 527
Tensile Modulus 2.35 GPa341 ksi1 mm/min; ISO 527
Flexural Strength 82.0 MPa11900 psi2mm/min; ISO 178
Flexural Modulus 2.30 GPa334 ksi2mm/min; ISO 178
Poissons Ratio 0.340.341mm/min; ISO 527
Charpy Impact, Notched  3.20 J/cm²
@Temperature -30.0 °C
15.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C252 °F120°C/h; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °F120°C/h; ISO 75
Vicat Softening Point 122 °C
@Load 5.00 kg
252 °F
@Load 11.0 lb
50°C/h; ISO 306
Flammability Test 29
@Thickness 3.00 mm
29
@Thickness 0.118 in
ISO 3795
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 255 °C410 - 491 °F
Middle Barrel Temperature 215 - 260 °C419 - 500 °F
Front Barrel Temperature 225 - 275 °C437 - 527 °F
Nozzle Temperature 230 - 275 °C446 - 527 °F
Melt Temperature 230 - 275 °C446 - 527 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 100 - 110 °C
@Time 14400 sec
212 - 230 °F
@Time 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %
Injection Pressure 70.0 - 110 MPa10200 - 16000 psi
Back Pressure 0.350 - 0.700 MPa50.8 - 102 psi
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEL00894 / 250016

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.