MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik POLYVEST® MA 75 Liquid
Categories: Other Engineering Material

Material Notes: POLYVEST® MA 75 is a maleic anhydride adduct of a low molecular weight 1,4-cis polybutadiene which as succinic anhydride groups randomly distributed along the polymer chains. This makes the originally apolar polybutadiene more polar and accessible for various chemical reactions.

General Use and Applications: Due to its high content of 1,4-cis double bonds the a polar, hydrophobic hydrocarbon resin POLYVEST MA 75 is a highly reactive binder featuring the following characteristics:

  • high chemical resistance
  • high water resistance
  • high electrical insulation properties
  • high cold resistance
  • good solubility in alphatic, aromatics and ethers
  • good compatibility with hydrocarbon resins, rosin resins and zinc resonates
In this form POLYVEST MA 75 is used in the following areas of application:
  • adhesive and sealant compositions
  • electrical insulations and potting compounds (2pack systems)
  • polymeric chalk activator in EPDM-compounds
  • modifier in carbon black filled EPDM-compounds
  • modifier in silica filled rubber compounds
  • modifier in rubber compounds for car tires
  • modifier in silicone sealants

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccDIN ISO 2811-1
Viscosity 6000 - 9000 cPDIN EN ISO 3219
Molecular Weight 3000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 70 - 90[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Pour Point -25.0 °CDIN ISO 3016
Flash Point 300 °CDIN EN ISO 2719
Ignition Temperature 360 °CDIN 51 794
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 2.5DIN ISO 4630
 
Descriptive Properties
Iodine No.380-420 g Iod/100gDIN 53 241

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik POLYVEST® MA 75 Polybutadienes

PEVONIM113 / 197317

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.