MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Pharmalene® MP 20 PH Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Pharmalene MP 20 PH is a medium fluidity low density polyethylene (LDPE) without additives, obtained by high pressure autoclave process. It is produced according to good manufacturing practices (GMP) and is mainly used for injection molding and extrusion coating.

Application: Pharmalene MP 20 PH is intended for the use within pharmaceutical sector and is characterized by high flexibility, excellent organoleptic properties and medium flow ability. Pharmalene MP 20 PH is suitable for the production of flexible medical packaging, pharmaceutical master batches and caps & closures.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccISO 1183
Thickness <= 10.0 micronsExtrusion coating processing
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48Injection Molded; ISO 868 A
Film Tensile Strength at Yield, MD 10.0 MPaISO 527-3
Flexural Modulus 130 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 108 °CManufacturer method
Vicat Softening Point 88.0 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -75.0 °CASTM D 746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 200 °CInjection Molding
 230 - 260 °CExtrusion coating
Mold Temperature 10.0 - 30.0 °CInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9862 / 265656

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.