Product Description: Escor 5020 is primarily intended for extrusion coating and coextrusion coating. Very good adhesion to polar substrates, aluminum foil, metalized films, papers, iron, steel and glass. Offers excellent balance of adhesion onto the substrates and interlayer adhesion with coextruded LDPE and EVA’s. Availability: Africa & Middle East, Asia Pacific and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: No
Applications:- Cable Shielding
- Coextrusion Coating
- Cosmetic Packaging
- Extrusion Coating
- Extrusion Lamination
- Food packaging
- Hygiene Packaging
- Lami Tubes
- Liquid Packaging
Information provided by ExxonMobil |