MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel

Material Notes: Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinability

Characteristics: Excellent machinability compared to conventional 4150 press brake tooling material

Applications: Brake Die

Hardening (Heat Treatment): 1544°F-1598°F; Cooling: Oil; Hardness: <51 HRC

Information provided by Schmolz + Bickenbach

Key Words: DIN 1.2312
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.283 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 28
@Treatment Temp. 700.0 °C
 36
@Treatment Temp. 600.0 °C
 42
@Treatment Temp. 500 °C
 46
@Treatment Temp. 400 °C
 48
@Treatment Temp. 300 °C
 50
@Treatment Temp. 200 °C
 51
@Treatment Temp. 100 °C
Tensile Strength 134 ksi32 HRC
 123 ksi
@Treatment Temp. 700.0 °C
28 HRC
 165 ksi
@Treatment Temp. 600.0 °C
36 HRC
 193 ksi
@Treatment Temp. 500 °C
42 HRC
 215 ksi
@Treatment Temp. 400 °C
46 HRC
 228 ksi
@Treatment Temp. 300 °C
48 HRC
 242 ksi
@Treatment Temp. 200 °C
50 HRC
 251 ksi
@Treatment Temp. 100 °C
51 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.80 µin/in-°F
@Temperature 21.1 - 93.3 °C
 7.20 µin/in-°F
@Temperature 21.1 - 204 °C
 7.60 µin/in-°F
@Temperature 21.1 - 302 °C
Thermal Conductivity 270 BTU-in/hr-ft²-°F
@Temperature 302 °C
 276 BTU-in/hr-ft²-°F
@Temperature 100 °C
 280 BTU-in/hr-ft²-°F
@Temperature 204 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1310 - 1365 °FSoft; Cooling: Furnace; < 235 HB
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 1.9 %
Iron, Fe 95.95 %
Manganese, Mn 1.5 %
Molybdenum, Mo 0.20 %
Sulfur, S 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Aluminum 5083-O
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C

NSCHMO024 / 125897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.