Varcum 29461 is a one-step liquid phenolic resin in methyl ethyl ketone. APPLICATION: General purpose resin used in nitrile rubber adhesive systems. FEATURES: - Excellent compatibility with both high and medium acrylonitrile content elastomers.
- Adhesives based on 29461 exhibit high strength metal to metal bonds.
- Contributes good heat and oil resistance to the adhesive.
- Contributes light color and resistance to staining effects upon exposure to ultraviolet light.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |