Dry as molded. Extrusion grade. Nylene NX4001A is a high viscosity, nucleated, nylon 6 extrusion grade resin. Crystallization initiators provide rapid melt set-up in higher speed processing applications. Optimum
processing conditions should provide a melt temperature of 550 - 575ºF at the die. Data provided by the manufacturer |