MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cosmic Plastics EH81 Epoxy, Iron-Filled, Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: Description: Cosmic EH81 is an iron-filled epoxy molding compound which is supplied in a black granular form.

Features: This material flows easily under low pressure and provides good moldability.

Applications: This material is good for EMI / RFI shielding, and can be either compression or transfer molded to fabricate core rods, or to encapsulate surface mount and axial leaded inductors. This single molded compound eliminates the labor intensive over/under molding.

Test Conditions: 1 MHz; 1/16" Rod; 0.008" wire; 25 No. of Turns

Data provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.50 g/cc
Density 3.60 g/cc
Spiral Flow 30.0 - 45.0 cm
Storage Temperature 5.00 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 130 - 180 °C
Shelf Life 4.00 Month
 
Descriptive Properties
Inductance0.43 – 0.50 Ls (uH)
Molding Pressure50 – 800 psi
Quality Factor7.3 – 9.5
Recommended Post Cure2-4 hrs@ 160°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAESCRh / 324931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.