  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnapas® AF 474 Polymer Dispersion
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® AF 474 is an aqueous dispersion of a hydroxy-functional acrylate copolymer.

Properties: VINNAPAS® AF 474 adheres extremely well to metals and many polar plastics and forms a transparent coating at room temperature. The dispersion's thermoplastic properties make it heat sealable. However if crosslinked with suitable reactants via the hydroxyl group VINNAPAS® AF 474 forms films that resist heat-sealing even at high temperatures.

Application: VINNAPAS® AF 474 is used for coating plastics, for rendering films heat sealable and, preferably in combination with melamine resins, for producing heat seal-resistant coatings with good water resistance, especially on aluminum foil. Depending on the formulation, VINNAPAS® AF 474 imparts heat-seal resistance up to 250 °C. Coatings based on VINNAPAS® AF 474 offer excellent printability. VINNAPAS® AF 474 substrates are especially suitable for printing with aqueous, acrylate-based printing-ink systems but as well with NC- or UV-inks. VINNAPAS® AF 474 is processed with conventional film-coating equipment, such as doctor blade or roller coaters. Drying conditions depend on the substrate's heat stability and on the final application where the polymers in VINNAPAS® AF 474 must remain thermoplastic, for example, or be crosslinked. Drying is normally at temperatures of up to 200 °C for a maximum of 20 minutes. Preliminary tests are needed to check the impact of additives, such as crosslinkers, on the heat stability of VINNAPAS® AF 474.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³DIN EN ISO 2881-1
Solids Content 44 - 46 %44 - 46 %DIN EN ISO 3251
Particle Size 0.10 µm0.10 µm
pH 7.5 - 8.57.5 - 8.5DIN/ISO 976
Viscosity 50 - 350 cP50 - 350 cPdynamic; DIN EN ISO 2555
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiDIN EN ISO 527-3
Elongation at Break 130 %130 %DIN EN ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 24.0 °C75.2 °F
 
Descriptive Properties
Content0.5-0.7%OH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013M-07 Cyclic Olefin Copolymer (COC)

PWACK9622 / 205151

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.