MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellamid® GS25-66 22L-NBK1 Nylon 66, 25% Glass Sphere
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Bead Filled

Material Notes: All Wellamid® and Techyer® grades feature excellent strength and stiffness with outstanding chemical and heat resistance. These products are used in automotive, lawn and garden, consumer and electronic applications.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183-87
Filler Content 25 %25 %Glass Sphere; ISO 3451
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/inDIS 294-4
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inDIS 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.0 MPa10200 psiISO 527-93
Elongation at Break 3.0 %3.0 %ISO 527-93
Flexural Strength 114 MPa16500 psiISO 178-93
Flexural Modulus 3.90 GPa566 ksiISO 178-93
Izod Impact, Notched (ISO) 3.30 kJ/m²1.57 ft-lb/in²ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FISO 75-93
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 266 - 293 °C511 - 559 °F
Middle Barrel Temperature 260 - 293 °C500 - 559 °F
Front Barrel Temperature 260 - 293 °C500 - 559 °F
Nozzle Temperature 254 - 293 °C489 - 559 °F
Melt Temperature 271 - 293 °C520 - 559 °F
Mold Temperature 71.0 - 93.0 °C160 - 199 °F
Injection Pressure 34.0 - 138 MPa4930 - 20000 psi
Back Pressure 0.340 - 1.03 MPa49.3 - 149 psi
Screw Speed 30 - 120 rpm30 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEL00857 / 249981

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.