MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® ZHF 90AT8 NAT 01 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Estane® ZHF 90AT8 NAT 01 is a non-halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane.

Application: Extrusion

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8989ISO 868
Tensile Strength 28.5 MPa4130 psiISO 527-2/5A/500
Elongation at Break 512 %512 %ISO 527-2/5A/500
50% Modulus 7.00 MPa
@Strain 50 %
7.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 11.0 MPa
@Strain 300 %
1600 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 54.5 kN/m311 pliNicked; ISO 34-1B
Abrasion 3838[mm3]; ISO 4649-A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 97.0 °C207 °FA50; ISO 306
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Zone 1 180 °C356 °F
Zone 2 185 °C365 °F
Zone 3 185 °C365 °F
Zone 4 190 °C374 °F
Adapter Temperature 195 °C383 °F(5)
Die Temperature 190 °C374 °FTIP (7)
 195 °C383 °F(6)
Drying Temperature 100 °C
@Time 10800 - 14400 sec
212 °F
@Time 3.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 24 %24 %ASTM D-2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5029 / 238899

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.