MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Butyl Rubber (IIR, CIIR, BIIR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and can improve adhesion.

IIR rubber resists degradation by fats/oils/greases and ozone and other strong oxidizing chemicals. IIR rubber is attacked by petrochemical solvents including aromatics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.35 g/cc0.0415 - 0.0488 lb/in³Compounded
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 35 - 9535 - 95Depends on compounding
Tensile Strength, Ultimate 17.0 MPa2470 psiCompounded Tire
Elongation at Break 400 - 800 %400 - 800 %
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 24.0 kV/mm610 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -25.0 °C-13.0 °F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
ATG s.r.l. IIR Butyl Rubber
Precision Polymer Engineering J70M Butyl Rubber
Sibur BK-1675N Butyl Rubber (IIR)

P0RU06 / 20055

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.