MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dover Chemical PAROIL 63NR Chlorinated Olefin Extreme Pressure Additive, Flame Retardant, Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Paroil 63-NR is a chlorinated compound. It is a nonflammable, non-corrosive, low volatile liquid at room temperature. It contains a stabilizer to maintain product integrity during transport and storage. Paroil 63-NR is used in a wide variety of applications including flame retardants, plasticizers and EP metalworking packages. For metalworking applications, Paroil 63-NR is typically (but not limited to) applied in straight oil machining, drawing, and stamping fluids.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
@Temperature 25.0 °C
Density 11.7 lb/gal
Viscosity 45000 cP
@Temperature 25.0 °C
Saybolt Viscosity at 210°F 310 SUS
ASTM Color 0.50
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 230 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 62 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER089 / 217708

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.