MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ovako 21CrMoV5-7 Imanite (6132) Steel, +QT
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: 21CrMoV5-7 is a steel for fasteners with specified elevated and/or low temperature properties. Imanite has been designed for nitriding, giving similar hardness distribution as case hardening. When using nitriding the distortion due to quenching after carburising can be avoided. Imanite is a M-steel version of 21CrMoV5-7 . M-treatment is very beneficial when the machining is done in Q&T condition and the hardness is about 300 HBW.

Information provided by Ovako

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 280 - 345
@Thickness 25.0 - 160 mm
Round bar
Tensile Strength 900 - 1100 MPa
@Thickness 25.0 - 160 mm
Round bar
Tensile Strength, Yield >= 800 MPa
@Thickness 25.0 - 160 mm
Round bar
Elongation at Break 14 %
@Thickness 25.0 - 160 mm
Round bar
Reduction of Area 60 %
@Thickness 25.0 - 160 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 35.0 J
@Thickness 25.0 - 160 mm,
Temperature 20.0 °C
Round bar, long
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 405 °CMS
 745 °CAC1
 853 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Calcium, Ca >= 0.0020 %
Carbon, C 0.17 - 0.25 %
Chromium, Cr 1.2 - 1.5 %
Iron, Fe 95.83 - 97.2 %As Balance
Manganese, Mn 0.35 - 0.85 %
Molybdenum, Mo 0.65 - 0.80 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S 0.025 - 0.040 %
Vanadium, V 0.25 - 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6082-T6
Ovako 32CrMoV12-10* 398Q Steel, Hardening
Ovako 40CrMoV4-6 6098 Steel, +QT
Ovako 42CrMo4 SB 9288 Steel, Quench & Tempering
Ovako 34CrMo4 SAE4130m Steel, +AR

NOVAKO169 / 234468

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.