MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sipol Technipol® PA 2126 Thermoplastic Adhesive Co-polyamide
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Technipol® PA 2126 is a co-polyamide hot-melt adhesive with a quick setting time and low application temperature. This co-polyamide adhesive has been mainly developed for engine air filters whose filtering media does not need to pass through curing ovens. Technipol® PA 2126 contains around 70 % of raw materials coming from renewable resources (non edible).

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D 792
Viscosity  2.0 cP
@Temperature 220 °C
2.0 cP
@Temperature 428 °F
 3.5 cP
@Temperature 200 °C
3.5 cP
@Temperature 392 °F
 7.0 cP
@Temperature 180 °C
7.0 cP
@Temperature 356 °F
 16 cP
@Temperature 160 °C
16 cP
@Temperature 320 °F
Brookfield Viscosity 5.0 cP
@Temperature 190 °C
5.0 cP
@Temperature 374 °F
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Storage Temperature 5.00 - 10.0 °C41.0 - 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 131 °C268 °FASTM D 3461
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorAmber
Suggested temperature profile for melters170-180°CPre-Heating Grills
 175-185°CTank
 175-185°CHose
 180-190°CNozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPOL014 / 297139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.