MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Rock Drill Oil ISO Grade 220
Categories: Fluid; Lubricant

Material Notes: Rock Drill Oil is an adhesive, extreme-pressure (EP) lubricant specially developed for the lubrication of air-powered tools such as rock drills, jackhammers, pavement breakers and drifters. It also is recommended for the lubrication of mining and industrial equipment operating in wet environments. Rock Drill Oil is formulated with high-quality paraffinic base oils and a specially tailored additive package to provide excellent protection for pneumatic percussion tools. It has high load-carrying capacity to protect against wear and seizure of sliding metal surfaces under heavy or shock-load conditions. It has good adhesion to metal surfaces in the presence of moisture, and provides protection against rust and corrosion. It also has good oxidation resistance and thermal stability at high temperatures for long service life.

Applications:

  • Pneumatic percussion tools such as jackhammers, pavement breakers and rock drills
  • Mining equipment such as demolition hammers, chipping hammers and drifters
  • Enclosed industrial gearboxes where leakage is a problem
Features/Benefits:
  • Non-chlorinated additive package for reduced environmental impact
  • Excellent extreme-pressure properties
  • Protects against wear and seizure
  • Good adhesion to metal surfaces in the presence of moisture
  • Resists dripping and leakage
  • Good oxidation resistance and thermal stability
  • Low odor
  • Good foam resistance
  • Eight viscosity grades for use over a wide range of temperatures

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.886 g/cc0.886 g/cc
Density 0.884 g/cc0.0319 lb/in³
Viscosity Measurement 106106Index
Saybolt Viscosity at 100°F 1158 SUS1158 SUS
Saybolt Viscosity at 210°F 102 SUS102 SUS
Kinematic Viscosity at 40°C (104°F) 220 cSt220 cSt
Kinematic Viscosity at 100°C (212°F) 20.2 cSt20.2 cSt
ASTM Color 3.53.5ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.680.68[mg KOH/g]; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)ASTM D2596
Four Ball Wear 0.370 mm0.0146 inScar Diameter; ASTM D4172
Falex Load Test 1.916e+6 g4225 lbASTM D3233
Timken Test 31700 g70.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Pour Point -18.0 °C-0.400 °F
Flash Point 234 °C453 °FCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5214 / 198467

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.