MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond F113SC High Tg Fiber Optic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F113SC is a room temperature curing, high Tg and low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors. It has also been used for bonding LED displays, lenses and other optical components. TRA-BOND F113SC provides both high bond strength as well as low stress connections with no pistoning. This two part system can be cured overnight at room temperature or as quickly as 15 minutes at 90°C and is provided in a dark blue color to allow for easy polishing. Sufficient cure is developed for polishing connectors in 15 minutes at 65°C, when higher cure temperatures are possible. TRA-BOND F113SC will complete its cure at room temperature with no pistoning.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccMixed
Volatile Organic Compounds (VOC) Content 1.91 g/l1.91 g/l
Water Absorption 0.98 %0.98 %
Viscosity 1800 cP
@Temperature 25.0 °C
1800 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Adhesive Bond Strength 18.6 MPa2700 psiLap shear, alum to alum, 24 hrs @ 25°C
 26.9 MPa3900 psiLap shear, alum to alum, 1 hr @ 65°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.7 µm/m-°C42.1 µin/in-°FBelow Tg
 191 µm/m-°C106 µin/in-°FAbove Tg
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 95.0 °C203 °FUltimate Tg
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.521.52
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 90.0 °C
0.250 hour
@Temperature 194 °F
1 drop applications
 60.0 min
@Temperature 65.0 °C
1.00 hour
@Temperature 149 °F
 1080 min
@Temperature 25.0 °C
18.0 hour
@Temperature 77.0 °F
Pot Life 35 min35 min25 grams
Working Life 60.0 min60.0 min25 grams
 
Descriptive Properties
Color ClearResin
 Dark BlueHardener/Mixed
Mix Ratio, parts by weight100/30Resin/Hardener
Thixotropic Index 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC226 / 71154

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.