Shielding - Stainless Steel Fiber 15% - 80 Shore A Comments: - EMI/RFI Shielding
- ESD Protection
- Stainless Steel Fiber
- 80-A Durometer
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |