MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt PREMABRAZE® 402 Gold-Copper Braze Alloy (AWS BVAu-10)
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Premabraze 402 can be used on any of the common ferrous and non-ferrous alloys. This alloy exhibits good wetting characteristics on metallized ceramics. Typical applications include brazing of electron tubes, vacuum tubes, radar devices, and wave guides in the electronic industry. Premabraze 402 is readily used in the brazing of ceramic to metal seals. Premabraze 402 is generally used in reducing, vacuum, or inert atmospheres. It is a less ductile alloy than standard gold-copper-nickel alloys. The composition of the alloy allows for use in applications where braze filler metals low in volatile constituents are required. Due to its narrow plastic range, Premabraze 402 exhibits free flowing characteristics.

Available forms: Wire, strip, engineered preforms, specialty preforms, powder and paste.

Information provided by Lucas-Milhaupt.

Key Words: AWS A5.8M/A5.8 BVAu-10 Grades 1 & 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 12.22 g/cc
Density 0.442 lb/in³
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000237 ohm-cm7.87% IACS
 
Thermal PropertiesOriginal ValueComments
Melting Point 1751 - 1778 °F
Solidus 1751 °F
Liquidus 1778 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1778 - 1868 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd <= 0.0010 %
Carbon, C <= 0.0050 %
Copper, Cu 49.47 - 50.47 %Remainder
Gold, Au 49.5 - 50.5 %
Lead, Pb <= 0.0020 %
Other, each <= 0.0010 %High vapor pressure elements.
Other, total <= 0.010 %high vapor pressure elements (Including zinc, cadmium, and lead)
 <= 0.010 %Impurity elements
Phosphorus, P <= 0.0020 %
Zinc, Zn <= 0.0010 %
 
Descriptive Properties
ColorRed brass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9830 / 254775

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.