DriscoPlex® 6300 Pipe meets or exceeds: ASTM F2619 API 15LE ASTM D3350, cell classification PE445574C PPI TR-4 designation PE4710 Iron Pipe Size OD (IPS) ¾” to 54”, 40’ and 50’ Joints / Solid Black Coils available in sizes through 6” DriscoPlex® 6300 Pipe for: Oil and Gas Gathering Sour Gas Raw Water and Brine Water Produced Water Multiphase Oilfield Solutions Non-Potable Oilfield Water Applications Not intended for regulated gas gathering applications Information provided by Chevron Phillips Chemical Company LP. |